Pentlandite Rajamani V, Prewitt C T American Mineralogist 60 (1975) 39-48 Thermal expansion of the pentlandite structure Outokumpu, at 235 deg C _database_code_amcsd 0000441 CELL PARAMETERS: 10.0040 10.0040 10.0040 90.000 90.000 90.000 SPACE GROUP: Fm3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 1001.200 Density (g/cm3): 5.191 MAX. ABS. INTENSITY / VOLUME**2: 75.62851991 RIR: 4.744 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 15.34 26.14 5.7758 1 1 1 8 17.73 4.92 5.0020 2 0 0 6 25.18 5.40 3.5369 2 2 0 12 29.62 95.13 3.0163 3 1 1 24 30.97 20.96 2.8879 2 2 2 8 35.91 7.86 2.5010 4 0 0 6 39.25 16.13 2.2951 3 3 1 24 40.32 3.29 2.2370 4 2 0 24 44.36 1.81 2.0421 4 2 2 24 47.21 28.77 1.9253 5 1 1 24 47.21 6.01 1.9253 3 3 3 8 51.69 100.00 1.7685 4 4 0 12 54.25 4.76 1.6910 5 3 1 48 60.71 9.40 1.5256 5 3 3 24 61.48 5.64 1.5082 6 2 2 24 64.54 1.63 1.4440 4 4 4 8 66.78 2.53 1.4008 7 1 1 24 72.59 6.11 1.3024 5 5 3 24 72.59 7.56 1.3024 7 3 1 48 76.12 12.35 1.2505 8 0 0 6 78.21 2.69 1.2222 7 3 3 24 83.73 5.95 1.1552 7 5 1 48 83.73 1.57 1.1552 5 5 5 8 84.41 2.03 1.1475 6 6 2 24 87.14 1.53 1.1185 8 4 0 24 89.19 1.95 1.0981 7 5 3 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.