Grossular Meagher E P American Mineralogist 60 (1975) 218-228 The crystal structures of pyrope and grossularite at elevated temperatures T = 365 deg C garnet _database_code_amcsd 0000451 CELL PARAMETERS: 11.8800 11.8800 11.8800 90.000 90.000 90.000 SPACE GROUP: Ia-3d X-RAY WAVELENGTH: 1.541838 Cell Volume: 1676.677 Density (g/cm3): 3.568 MAX. ABS. INTENSITY / VOLUME**2: 24.60730506 RIR: 2.245 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 30.09 35.73 2.9700 4 0 0 6 33.74 100.00 2.6564 4 2 0 24 35.44 6.75 2.5328 3 3 2 24 37.07 18.30 2.4250 4 2 2 24 38.65 14.23 2.3299 4 3 1 48 41.64 12.81 2.1690 5 2 1 48 43.07 3.07 2.1001 4 4 0 12 47.16 9.85 1.9272 5 3 2 48 47.16 11.19 1.9272 6 1 1 24 48.46 1.42 1.8784 6 2 0 24 53.43 14.17 1.7147 4 4 4 8 55.80 24.08 1.6475 6 4 0 24 56.96 1.10 1.6167 5 5 2 24 58.10 38.88 1.5875 6 4 2 48 62.55 8.89 1.4850 8 0 0 6 63.63 1.54 1.4623 7 4 1 48 70.96 8.80 1.3282 8 4 0 24 72.99 14.76 1.2962 8 4 2 48 75.00 5.98 1.2664 6 6 4 24 79.94 1.68 1.2001 9 4 1 48 79.94 1.78 1.2001 8 5 3 48 82.87 1.54 1.1649 10 2 0 24 88.68 4.71 1.1030 10 4 0 24 88.68 8.00 1.1030 8 6 4 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.