Armalcolite Wechsler B A American Mineralogist 62 (1977) 913-920 Cation distribution and high-temperature crystal chemistry of armalcolite sample Arm-E, T = 24 deg C, after heating _database_code_amcsd 0000593 CELL PARAMETERS: 9.7697 10.0410 3.7473 90.000 90.000 90.000 SPACE GROUP: Bbmm X-RAY WAVELENGTH: 1.541838 Cell Volume: 367.601 Density (g/cm3): 3.897 MAX. ABS. INTENSITY / VOLUME**2: 25.19052075 RIR: 2.105 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 17.67 12.37 5.0205 0 2 0 2 18.16 36.65 4.8849 2 0 0 2 20.22 2.33 4.3926 2 1 0 4 25.44 7.89 3.5011 2 2 0 4 25.46 100.00 3.4988 1 0 1 4 26.99 3.77 3.3039 1 1 1 8 31.16 4.24 2.8705 1 2 1 8 32.43 70.09 2.7611 2 3 0 4 36.56 17.87 2.4581 3 0 1 4 36.80 5.84 2.4424 4 0 0 2 37.17 19.96 2.4186 1 3 1 8 37.68 1.72 2.3876 3 1 1 8 40.40 13.45 2.2327 2 4 0 4 40.88 1.27 2.2077 3 2 1 8 41.10 15.32 2.1963 4 2 0 4 45.80 4.35 1.9812 3 3 1 8 46.00 18.87 1.9730 4 3 0 4 48.59 31.67 1.8736 0 0 2 2 49.05 9.92 1.8574 2 5 0 4 52.07 8.17 1.7563 3 4 1 8 52.29 3.16 1.7494 2 0 2 4 53.68 1.56 1.7073 5 1 1 8 54.86 12.04 1.6735 0 6 0 2 55.64 1.37 1.6520 2 2 2 8 56.16 17.23 1.6378 5 2 1 8 56.52 1.68 1.6283 6 0 0 2 57.32 3.85 1.6073 6 1 0 4 58.28 2.84 1.5832 2 6 0 4 59.43 7.89 1.5552 3 5 1 8 59.64 18.76 1.5504 2 3 2 8 60.14 15.71 1.5386 5 3 1 8 61.41 5.37 1.5097 1 6 1 8 62.47 2.24 1.4866 4 0 2 4 63.54 2.02 1.4642 6 3 0 4 64.98 4.28 1.4352 2 4 2 8 65.46 2.71 1.4259 5 4 1 8 65.48 5.77 1.4254 4 2 2 8 67.74 5.37 1.3833 3 6 1 8 67.89 1.05 1.3805 4 6 0 4 68.13 1.94 1.3763 2 7 0 4 69.14 7.74 1.3586 4 3 2 8 71.02 1.58 1.3272 1 7 1 8 71.53 4.60 1.3191 2 5 2 8 72.94 4.02 1.2969 7 1 1 8 75.05 6.20 1.2657 7 2 1 8 75.11 1.68 1.2648 6 5 0 4 76.29 6.76 1.2481 0 6 2 4 76.95 2.39 1.2390 1 0 3 4 77.70 1.02 1.2290 6 0 2 4 78.39 2.48 1.2199 6 1 2 8 79.21 1.73 1.2093 2 6 2 8 81.04 1.36 1.1866 8 2 0 4 82.76 1.45 1.1663 3 0 3 4 83.13 1.91 1.1620 1 3 3 8 83.86 1.50 1.1537 6 3 2 8 87.35 2.40 1.1163 4 8 0 4 88.06 1.58 1.1092 2 7 2 8 89.40 2.14 1.0960 7 5 1 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.