Tausonite Yamanaka T, Hirai M, Komatsu Y American Mineralogist 87 (2002) 1183-1189 Structure change of Ca1-xSrxTiO3 perovskite with composition and pressure Sample: Ca.4Sr.6TiO3, x = 0.6 _database_code_amcsd 0002893 CELL PARAMETERS: 5.4784 5.4791 7.7517 90.000 90.000 90.000 SPACE GROUP: Pbnm X-RAY WAVELENGTH: 1.541838 Cell Volume: 232.680 Density (g/cm3): 4.694 MAX. ABS. INTENSITY / VOLUME**2: 77.94987140 RIR: 5.407 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 32.68 79.85 2.7400 1 1 2 8 32.69 20.15 2.7396 0 2 0 2 32.69 20.17 2.7392 2 0 0 2 40.31 9.75 2.2371 0 2 2 4 40.32 9.80 2.2369 2 0 2 4 46.88 15.92 1.9379 0 0 4 2 46.91 33.21 1.9370 2 2 0 4 58.32 7.21 1.5821 0 2 4 4 58.33 7.22 1.5820 2 0 4 4 58.34 13.34 1.5818 1 3 2 8 58.34 13.40 1.5816 3 1 2 8 68.49 15.31 1.3700 2 2 4 8 68.50 3.95 1.3698 0 4 0 2 68.51 3.98 1.3696 4 0 0 2 77.96 5.07 1.2256 1 1 6 8 77.99 4.95 1.2251 3 3 2 8 77.99 2.57 1.2251 2 4 0 4 78.00 2.59 1.2250 4 2 0 4 82.59 1.24 1.1682 2 4 2 8 82.60 1.26 1.1681 4 2 2 8 87.13 3.33 1.1186 0 4 4 4 87.14 3.36 1.1185 4 0 4 4 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.