(K.6Na.4)Cl Walker D, Verma P K, Cranswick L M D, Jones R L, Clark S M, Buhre S American Mineralogist 89 (2004) 204-210 Halite-sylvite thermoelasticity Sample: als8k60, T = 650 C, P = 0.0 kbar, cell volume = 245.25 ang**3 _database_code_amcsd 0003296 CELL PARAMETERS: 6.2595 6.2595 6.2595 90.000 90.000 90.000 SPACE GROUP: Fm3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 245.256 Density (g/cm3): 1.844 MAX. ABS. INTENSITY / VOLUME**2: 30.03526674 RIR: 5.303 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 28.52 100.00 3.1298 2 0 0 6 40.77 63.88 2.2131 2 2 0 12 50.51 19.70 1.8070 2 2 2 8 59.03 8.17 1.5649 4 0 0 6 66.84 20.33 1.3997 4 2 0 24 74.22 13.81 1.2777 4 2 2 24 88.33 3.96 1.1065 4 4 0 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.