Ulvospinel Bosi F, Halenius U, Skogby H American Mineralogist 94 (2009) 181-189 Crystal chemistry of the magnetite-ulvospinel series Locality: synthetic Note: FeTi50C _database_code_amcsd 0004823 CELL PARAMETERS: 8.4875 8.4875 8.4875 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 611.420 Density (g/cm3): 4.918 MAX. ABS. INTENSITY / VOLUME**2: 79.71883542 RIR: 5.278 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.10 8.00 4.9003 1 1 1 8 29.77 31.31 3.0008 2 2 0 12 35.07 100.00 2.5591 3 1 1 24 36.68 6.97 2.4501 2 2 2 8 42.61 19.16 2.1219 4 0 0 6 52.84 10.00 1.7325 4 2 2 24 56.32 26.80 1.6334 5 1 1 24 56.32 5.53 1.6334 3 3 3 8 61.84 40.75 1.5004 4 4 0 12 70.12 3.45 1.3420 6 2 0 24 73.11 8.36 1.2943 5 3 3 24 74.10 3.54 1.2795 6 2 2 24 78.00 2.31 1.2251 4 4 4 8 85.64 3.91 1.1342 6 4 2 48 88.48 7.39 1.1050 7 3 1 48 88.48 5.41 1.1050 5 5 3 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.