Ulvospinel Bosi F, Halenius U, Skogby H American Mineralogist 94 (2009) 181-189 Crystal chemistry of the magnetite-ulvospinel series Locality: synthetic Note: FeTib2 _database_code_amcsd 0004830 CELL PARAMETERS: 8.5220 8.5220 8.5220 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 618.906 Density (g/cm3): 4.824 MAX. ABS. INTENSITY / VOLUME**2: 77.64712848 RIR: 5.241 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.03 8.40 4.9202 1 1 1 8 29.65 32.51 3.0130 2 2 0 12 34.92 100.00 2.5695 3 1 1 24 36.52 6.80 2.4601 2 2 2 8 42.43 18.99 2.1305 4 0 0 6 52.61 10.40 1.7395 4 2 2 24 56.08 29.11 1.6401 5 1 1 24 56.08 5.36 1.6401 3 3 3 8 61.56 42.32 1.5065 4 4 0 12 69.80 3.61 1.3474 6 2 0 24 72.77 8.96 1.2996 5 3 3 24 73.75 3.96 1.2847 6 2 2 24 77.62 2.38 1.2300 4 4 4 8 85.21 4.39 1.1388 6 4 2 48 88.03 7.76 1.1095 7 3 1 48 88.03 6.10 1.1095 5 5 3 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.