Ulvospinel Bosi F, Halenius U, Skogby H American Mineralogist 94 (2009) 181-189 Crystal chemistry of the magnetite-ulvospinel series Locality: synthetic Note: FeTib1c _database_code_amcsd 0004832 CELL PARAMETERS: 8.5307 8.5307 8.5307 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 620.803 Density (g/cm3): 4.795 MAX. ABS. INTENSITY / VOLUME**2: 76.27140744 RIR: 5.179 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.01 8.43 4.9252 1 1 1 8 29.62 33.06 3.0161 2 2 0 12 34.88 100.00 2.5721 3 1 1 24 36.49 6.68 2.4626 2 2 2 8 42.38 18.77 2.1327 4 0 0 6 52.56 10.48 1.7413 4 2 2 24 56.01 29.43 1.6417 5 1 1 24 56.01 5.26 1.6417 3 3 3 8 61.49 42.13 1.5080 4 4 0 12 69.72 3.61 1.3488 6 2 0 24 72.68 8.94 1.3009 5 3 3 24 73.66 3.96 1.2861 6 2 2 24 77.53 2.32 1.2313 4 4 4 8 85.11 4.43 1.1400 6 4 2 48 87.92 6.10 1.1106 5 5 3 24 87.92 7.63 1.1106 7 3 1 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.