Tennantite Makovicky E, Karanovic L, Poleti D, Balic-Zunic T, Paar W H The Canadian Mineralogist 43 (2005) 679-688 Crystal structure of copper-rich unsubstituted tennantite, Cu12.5As4S13 Sample: Cerro Atajo, Catamarco, Argentina _database_code_amcsd 0006002 CELL PARAMETERS: 10.1756 10.1756 10.1756 90.000 90.000 90.000 SPACE GROUP: I-43m X-RAY WAVELENGTH: 1.541838 Cell Volume: 1053.610 Density (g/cm3): 4.782 MAX. ABS. INTENSITY / VOLUME**2: 102.9087295 RIR: 7.008 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 12.30 2.27 7.1952 1 1 0 12 21.39 3.43 4.1542 2 1 1 12 24.75 1.72 3.5976 2 2 0 12 30.43 100.00 2.9374 2 2 2 4 32.94 2.40 2.7195 3 2 1 24 35.28 16.34 2.5439 4 0 0 6 37.50 1.72 2.3984 4 1 1 12 37.50 3.12 2.3984 3 3 0 12 43.57 1.25 2.0771 4 2 2 12 45.45 3.34 1.9956 4 3 1 24 49.03 9.17 1.8578 5 2 1 24 50.75 41.34 1.7988 4 4 0 12 52.43 1.87 1.7451 4 3 3 12 55.68 1.14 1.6507 5 3 2 24 55.68 3.24 1.6507 6 1 1 12 57.26 1.27 1.6089 6 2 0 24 60.34 19.92 1.5340 6 2 2 12 63.32 2.41 1.4687 4 4 4 4 64.78 1.21 1.4390 7 1 0 24 74.61 3.72 1.2720 8 0 0 6 78.67 1.49 1.2162 6 5 3 24 81.34 1.02 1.1829 7 4 3 24 82.67 5.79 1.1672 6 6 2 12 85.32 1.74 1.1377 8 4 0 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.