Aragonite Antao S M, Hassan I The Canadian Mineralogist 48 (2010) 1225-1236 Temperature dependence of the structural parameters in the transformation of aragonite to calcite, as determined from in situ synchrotron powder X-ray-diffraction data Locality: Cuenca, Spain Note: T = 218 C Note: P = 101 kPa _database_code_amcsd 0017835 CELL PARAMETERS: 4.9644 8.0057 5.7805 90.000 90.000 90.000 SPACE GROUP: Pmcn X-RAY WAVELENGTH: 1.541838 Cell Volume: 229.737 Density (g/cm3): 2.893 MAX. ABS. INTENSITY / VOLUME**2: 10.19201549 RIR: 1.147 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 21.06 1.48 4.2191 1 1 0 4 22.21 1.79 4.0029 0 2 0 2 26.15 100.00 3.4079 1 1 1 8 27.10 51.84 3.2909 0 2 1 4 30.94 5.18 2.8902 0 0 2 2 32.65 7.52 2.7429 1 2 1 8 32.95 50.43 2.7185 0 1 2 4 35.95 18.08 2.4978 1 0 2 4 36.19 16.48 2.4822 2 0 0 2 37.11 9.87 2.4228 0 3 1 4 37.73 43.49 2.3844 1 1 2 8 38.29 26.96 2.3505 1 3 0 4 38.42 15.92 2.3433 0 2 2 4 41.15 11.82 2.1935 2 1 1 8 42.87 17.82 2.1095 2 2 0 4 45.31 3.21 2.0014 0 4 0 2 45.79 64.01 1.9817 2 2 1 8 48.11 27.20 1.8913 0 4 1 4 48.33 12.97 1.8831 2 0 2 4 49.74 1.92 1.8330 2 1 2 8 50.02 27.29 1.8236 1 3 2 8 51.72 1.88 1.7674 1 4 1 8 52.19 28.08 1.7527 1 1 3 8 52.72 11.68 1.7362 0 2 3 4 52.80 5.21 1.7338 2 3 1 8 53.80 3.12 1.7039 2 2 2 8 55.88 3.27 1.6454 0 4 2 4 56.81 1.74 1.6205 3 1 0 4 59.22 6.19 1.5604 3 1 1 8 59.31 1.74 1.5580 2 4 0 4 59.95 1.89 1.5430 0 5 1 4 61.66 4.84 1.5044 2 4 1 8 62.86 1.94 1.4784 3 2 1 8 63.09 6.76 1.4735 1 5 1 8 65.65 1.93 1.4221 0 1 4 4 66.10 3.52 1.4135 3 1 2 8 66.48 3.03 1.4064 3 3 0 4 68.40 3.26 1.3715 2 4 2 8 68.65 3.64 1.3671 1 1 4 8 69.11 1.82 1.3593 0 2 4 4 69.77 2.45 1.3480 1 5 2 8 70.59 1.81 1.3343 0 6 0 2 75.12 6.28 1.2646 3 3 2 8 76.24 3.99 1.2489 2 0 4 4 76.80 4.24 1.2411 4 0 0 2 76.87 7.35 1.2402 3 1 3 8 77.54 6.38 1.2311 1 3 4 8 79.04 5.86 1.2115 2 4 3 8 79.04 2.09 1.2114 0 6 2 4 80.33 5.69 1.1952 1 5 3 8 81.99 6.18 1.1752 2 6 0 4 83.19 3.01 1.1613 4 2 1 8 86.17 3.39 1.1285 3 5 1 8 87.48 2.14 1.1150 1 1 5 8 87.91 1.62 1.1107 0 2 5 4 89.32 1.17 1.0968 4 2 2 8 89.57 1.52 1.0943 1 7 1 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.