Aragonite Antao S M, Hassan I The Canadian Mineralogist 48 (2010) 1225-1236 Temperature dependence of the structural parameters in the transformation of aragonite to calcite, as determined from in situ synchrotron powder X-ray-diffraction data Locality: Cuenca, Spain Note: T = 318 C Note: P = 101 kPa _database_code_amcsd 0017840 CELL PARAMETERS: 4.9693 8.0234 5.8037 90.000 90.000 90.000 SPACE GROUP: Pmcn X-RAY WAVELENGTH: 1.541838 Cell Volume: 231.397 Density (g/cm3): 2.873 MAX. ABS. INTENSITY / VOLUME**2: 10.07005862 RIR: 1.141 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 21.03 1.56 4.2246 1 1 0 4 22.16 2.08 4.0117 0 2 0 2 26.09 100.00 3.4156 1 1 1 8 27.02 51.37 3.3000 0 2 1 4 30.81 4.53 2.9018 0 0 2 2 32.57 7.50 2.7491 1 2 1 8 32.82 48.69 2.7289 0 1 2 4 35.83 18.64 2.5059 1 0 2 4 36.15 16.20 2.4846 2 0 0 2 37.01 10.18 2.4290 0 3 1 4 37.60 44.34 2.3919 1 1 2 8 38.22 26.67 2.3550 1 3 0 4 38.28 15.67 2.3512 0 2 2 4 41.09 11.17 2.1968 2 1 1 8 42.81 17.65 2.1123 2 2 0 4 45.20 2.79 2.0059 0 4 0 2 45.71 61.01 1.9849 2 2 1 8 47.99 26.31 1.8958 0 4 1 4 48.22 12.12 1.8873 2 0 2 4 49.62 2.12 1.8372 2 1 2 8 49.87 26.21 1.8286 1 3 2 8 51.60 2.16 1.7713 1 4 1 8 51.99 26.97 1.7589 1 1 3 8 52.52 11.27 1.7425 0 2 3 4 52.70 4.73 1.7369 2 3 1 8 53.67 2.81 1.7078 2 2 2 8 55.71 3.35 1.6500 0 4 2 4 56.75 1.76 1.6222 3 1 0 4 59.13 5.77 1.5623 3 1 1 8 59.20 1.75 1.5607 2 4 0 4 59.79 1.89 1.5466 0 5 1 4 61.53 4.47 1.5072 2 4 1 8 62.76 1.96 1.4804 3 2 1 8 62.94 6.35 1.4768 1 5 1 8 65.36 2.04 1.4278 0 1 4 4 65.97 3.33 1.4160 3 1 2 8 66.38 2.71 1.4082 3 3 0 4 68.23 3.11 1.3745 2 4 2 8 68.36 3.28 1.3722 1 1 4 8 68.81 1.68 1.3644 0 2 4 4 69.57 2.32 1.3514 1 5 2 8 70.41 1.73 1.3372 0 6 0 2 74.96 5.77 1.2669 3 3 2 8 75.95 3.77 1.2529 2 0 4 4 76.66 6.77 1.2430 3 1 3 8 76.71 3.88 1.2423 4 0 0 2 77.23 5.77 1.2353 1 3 4 8 78.79 5.20 1.2147 2 4 3 8 78.81 1.81 1.2145 0 6 2 4 80.06 5.30 1.1986 1 5 3 8 81.79 5.57 1.1775 2 6 0 4 83.07 2.70 1.1627 4 2 1 8 85.99 3.10 1.1305 3 5 1 8 87.07 1.81 1.1193 1 1 5 8 87.48 1.46 1.1150 0 2 5 4 89.15 1.03 1.0984 4 2 2 8 89.32 1.31 1.0968 1 7 1 8 89.91 1.42 1.0911 2 6 2 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.