CoAl2O4 O'Neill H St C European Journal of Mineralogy 6 (1994) 603-609 Temperature dependence of the cation distribution in CoAl2O4 spinel Quenched from T = 950 C _database_code_amcsd 0006557 CELL PARAMETERS: 8.1069 8.1069 8.1069 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 532.796 Density (g/cm3): 4.410 MAX. ABS. INTENSITY / VOLUME**2: 46.48823750 RIR: 3.433 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 31.21 58.23 2.8662 2 2 0 12 36.77 100.00 2.4443 3 1 1 24 44.71 12.29 2.0267 4 0 0 6 48.98 3.70 1.8598 3 3 1 24 55.53 17.99 1.6548 4 2 2 24 59.22 4.37 1.5602 3 3 3 8 59.22 35.70 1.5602 5 1 1 24 65.09 48.00 1.4331 4 4 0 12 73.94 6.27 1.2818 6 2 0 24 77.16 10.01 1.2363 5 3 3 24 78.22 1.04 1.2222 6 2 2 24 82.42 1.22 1.1701 4 4 4 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.