CoAl2O4 O'Neill H St C European Journal of Mineralogy 6 (1994) 603-609 Temperature dependence of the cation distribution in CoAl2O4 spinel Quenched from T = 1000 C _database_code_amcsd 0006558 CELL PARAMETERS: 8.1063 8.1063 8.1063 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 532.682 Density (g/cm3): 4.411 MAX. ABS. INTENSITY / VOLUME**2: 46.07591088 RIR: 3.401 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 31.21 58.11 2.8660 2 2 0 12 36.77 100.00 2.4441 3 1 1 24 44.72 12.36 2.0266 4 0 0 6 48.98 3.63 1.8597 3 3 1 24 55.54 17.77 1.6547 4 2 2 24 59.23 4.31 1.5601 3 3 3 8 59.23 35.30 1.5601 5 1 1 24 65.09 47.32 1.4330 4 4 0 12 73.95 6.13 1.2817 6 2 0 24 77.16 9.78 1.2362 5 3 3 24 78.22 1.01 1.2221 6 2 2 24 82.43 1.19 1.1700 4 4 4 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.