Ulvospinel Sedler I K, Feenstra A, Peters T European Journal of Mineralogy 6 (1994) 873-885 An X-ray powder diffraction study of synthetic (Fe,Mn)2TiO4 spinel Sample: D-08 _database_code_amcsd 0006573 CELL PARAMETERS: 8.6112 8.6112 8.6112 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 638.544 Density (g/cm3): 4.631 MAX. ABS. INTENSITY / VOLUME**2: 66.14443703 RIR: 4.650 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 17.84 22.60 4.9717 1 1 1 8 29.34 24.03 3.0445 2 2 0 12 34.55 100.00 2.5964 3 1 1 24 36.13 10.33 2.4858 2 2 2 8 41.97 27.92 2.1528 4 0 0 6 45.94 1.16 1.9755 3 3 1 24 52.03 7.16 1.7578 4 2 2 24 55.44 5.10 1.6572 3 3 3 8 55.44 28.59 1.6572 5 1 1 24 60.85 42.26 1.5223 4 4 0 12 63.96 2.75 1.4556 5 3 1 48 68.97 2.38 1.3616 6 2 0 24 71.90 8.41 1.3132 5 3 3 24 72.86 5.38 1.2982 6 2 2 24 76.67 3.28 1.2429 4 4 4 8 79.48 1.15 1.2058 5 5 1 24 84.13 2.95 1.1507 6 4 2 48 86.89 5.51 1.1211 5 5 3 24 86.89 7.01 1.1211 7 3 1 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.