CdGeO3 Susaki J Physics and Chemistry of Minerals 16 (1989) 634-641 CdGeO3-phase transformations at high pressure and temperature and structural refinement of the perovskite polymorph _database_code_amcsd 0007463 CELL PARAMETERS: 5.2114 5.2608 7.4263 90.000 90.000 90.000 SPACE GROUP: Pbnm X-RAY WAVELENGTH: 1.541838 Cell Volume: 203.600 Density (g/cm3): 7.602 MAX. ABS. INTENSITY / VOLUME**2: 212.4308675 RIR: 9.099 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 23.97 1.60 3.7132 0 0 2 2 24.04 2.48 3.7024 1 1 0 4 26.91 3.21 3.3134 1 1 1 8 34.08 24.09 2.6304 0 2 0 2 34.20 100.00 2.6218 1 1 2 8 34.42 23.66 2.6057 2 0 0 2 36.23 1.78 2.4795 0 2 1 4 40.50 1.33 2.2275 2 1 1 8 42.10 4.16 2.1464 0 2 2 4 42.38 4.08 2.1329 2 0 2 4 44.00 1.53 2.0578 1 1 3 8 49.07 13.49 1.8566 0 0 4 2 49.22 24.99 1.8512 2 2 0 4 50.64 1.35 1.8027 0 2 3 4 50.83 2.15 1.7962 2 2 1 8 56.76 3.58 1.6219 1 3 1 8 61.09 15.27 1.5170 1 3 2 8 61.09 9.67 1.5168 0 2 4 4 61.31 9.77 1.5120 2 0 4 4 61.51 20.37 1.5075 3 1 2 8 67.93 1.65 1.3799 1 3 3 8 71.77 2.67 1.3152 0 4 0 2 72.04 12.27 1.3109 2 2 4 8 72.56 2.98 1.3029 4 0 0 2 73.07 1.01 1.2950 0 4 1 4 82.08 2.50 1.1741 2 4 0 4 82.10 7.10 1.1739 1 1 6 8 82.34 5.74 1.1711 3 3 2 8 82.65 2.94 1.1675 4 2 0 4 83.33 1.14 1.1597 2 4 1 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.