Magnetite O'Neill H St C, Dollase W A Physics and Chemistry of Minerals 20 (1994) 541-555 Crystal structures and cation distributions in simple spinels from powder XRD structural refinements: MgCr2O4, ZnCr2O4, Fe3O4 and the temperature dependence of the cation distribution in ZnAl2O4 Sample: 1B model, Fe3O4 Locality: synthetic _database_code_amcsd 0007781 CELL PARAMETERS: 8.3970 8.3970 8.3970 90.000 90.000 90.000 SPACE GROUP: Fd-3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 592.069 Density (g/cm3): 5.194 MAX. ABS. INTENSITY / VOLUME**2: 90.60518926 RIR: 5.680 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.30 8.76 4.8480 1 1 1 8 30.10 28.40 2.9688 2 2 0 12 35.46 100.00 2.5318 3 1 1 24 37.09 8.24 2.4240 2 2 2 8 43.09 20.43 2.0993 4 0 0 6 53.46 9.34 1.7140 4 2 2 24 56.99 25.28 1.6160 5 1 1 24 56.99 6.02 1.6160 3 3 3 8 62.58 41.21 1.4844 4 4 0 12 65.80 1.06 1.4194 5 3 1 48 70.99 3.32 1.3277 6 2 0 24 74.03 8.47 1.2805 5 3 3 24 75.03 3.75 1.2659 6 2 2 24 79.00 2.65 1.2120 4 4 4 8 86.79 3.66 1.1221 6 4 2 48 89.69 8.07 1.0932 7 3 1 48 89.69 5.36 1.0932 5 5 3 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.