Tungsten Dubrovinsky L S, Saxena S K Physics and Chemistry of Minerals 24 (1997) 547-550 Thermal expansion of periclase (MgO) and tungsten (W) to melting temperatures Sample: T = 1205 K _database_code_amcsd 0008072 CELL PARAMETERS: 3.1775 3.1775 3.1775 90.000 90.000 90.000 SPACE GROUP: Im3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 32.082 Density (g/cm3): 19.028 MAX. ABS. INTENSITY / VOLUME**2: 2242.812917 RIR: 38.379 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 40.13 100.00 2.2468 1 1 0 12 58.06 15.81 1.5888 2 0 0 6 72.92 29.64 1.2972 2 1 1 24 86.66 8.90 1.1234 2 2 0 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.