Tungsten Dubrovinsky L S, Saxena S K Physics and Chemistry of Minerals 24 (1997) 547-550 Thermal expansion of periclase (MgO) and tungsten (W) to melting temperatures Sample: T = 2032 K _database_code_amcsd 0008080 CELL PARAMETERS: 3.1926 3.1926 3.1926 90.000 90.000 90.000 SPACE GROUP: Im3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 32.541 Density (g/cm3): 18.760 MAX. ABS. INTENSITY / VOLUME**2: 2211.450726 RIR: 38.384 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 39.94 100.00 2.2575 1 1 0 12 57.76 15.85 1.5963 2 0 0 6 72.52 29.75 1.3034 2 1 1 24 86.15 8.91 1.1288 2 2 0 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.