Tungsten Dubrovinsky L S, Saxena S K Physics and Chemistry of Minerals 24 (1997) 547-550 Thermal expansion of periclase (MgO) and tungsten (W) to melting temperatures Sample: T = 2774 K _database_code_amcsd 0008086 CELL PARAMETERS: 3.2116 3.2116 3.2116 90.000 90.000 90.000 SPACE GROUP: Im3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 33.126 Density (g/cm3): 18.429 MAX. ABS. INTENSITY / VOLUME**2: 2172.714626 RIR: 38.389 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 39.69 100.00 2.2709 1 1 0 12 57.38 15.91 1.6058 2 0 0 6 72.03 29.88 1.3111 2 1 1 24 85.52 8.92 1.1355 2 2 0 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.