Monteponite Zhang J Physics and Chemistry of Minerals 26 (1999) 644-648 Room temperature compressibilities of MnO and CdO: further examination of the role of cation type in bulk modulus systematics Sample from Run #1: P = 5.41 GPa _database_code_amcsd 0008261 CELL PARAMETERS: 4.6433 4.6433 4.6433 90.000 90.000 90.000 SPACE GROUP: Fm3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 100.111 Density (g/cm3): 8.519 MAX. ABS. INTENSITY / VOLUME**2: 293.0211805 RIR: 11.200 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 33.42 100.00 2.6808 1 1 1 8 38.79 86.68 2.3217 2 0 0 6 56.02 50.21 1.6417 2 2 0 12 66.82 33.64 1.4000 3 1 1 24 70.22 14.72 1.3404 2 2 2 8 83.23 6.24 1.1608 4 0 0 6 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.