NaAl2(AlSi3)O11 Comodi P, Zanazzi P F Physics and Chemistry of Minerals 27 (2000) 377-385 Structural thermal behavior of paragonite and its dehydroxylate: a high-temperature single-crystal study Sample: Dehydroxylate phase at T = 25 C _database_code_amcsd 0008411 5.182 9.117 19.550 90 92.70 90 C2/c atom x y z occ Uiso Na 0 .0909 .25 .082 AlM2 .2774 .0937 .0002 .0228 AlT1 .9414 .4308 .1415 .25 .0232 SiT1 .9414 .4308 .1415 .75 .0232 AlT2 .4192 .2547 .1414 .25 .0250 SiT2 .4192 .2547 .1414 .75 .0250 O1 .9784 .4616 .0586 .025 O2 .3360 .2443 .0585 .027 O3 .3674 .0909 .1755 .030 O4 .7212 .3053 .1574 .034 O5 .2230 .3746 .1769 .030 Or 0 0 0 .055