Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: L-Cr, 3rd run, T = 600 C _database_code_amcsd 0008774 CELL PARAMETERS: 8.1335 8.1335 8.1335 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 538.062 Density (g/cm3): 3.555 MAX. ABS. INTENSITY / VOLUME**2: 18.31593617 RIR: 1.678 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.90 39.31 4.6959 1 1 1 8 31.10 32.98 2.8756 2 2 0 12 36.64 100.00 2.4523 3 1 1 24 44.56 57.52 2.0334 4 0 0 6 55.34 8.23 1.6602 4 2 2 24 59.01 2.65 1.5653 3 3 3 8 59.01 43.19 1.5653 5 1 1 24 64.85 67.40 1.4378 4 4 0 12 68.21 3.73 1.3748 5 3 1 48 73.66 2.26 1.2860 6 2 0 24 76.86 9.16 1.2403 5 3 3 24 77.91 1.03 1.2262 6 2 2 24 82.09 6.37 1.1740 4 4 4 8 85.20 3.07 1.1389 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.