Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: L-Cr, 3rd run, T = 700 C _database_code_amcsd 0008776 CELL PARAMETERS: 8.1423 8.1423 8.1423 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 539.810 Density (g/cm3): 3.544 MAX. ABS. INTENSITY / VOLUME**2: 18.34431296 RIR: 1.686 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.88 34.46 4.7010 1 1 1 8 31.07 32.08 2.8787 2 2 0 12 36.60 100.00 2.4550 3 1 1 24 44.51 55.37 2.0356 4 0 0 6 55.27 8.36 1.6620 4 2 2 24 58.94 3.03 1.5670 3 3 3 8 58.94 39.46 1.5670 5 1 1 24 64.77 64.31 1.4394 4 4 0 12 68.13 3.09 1.3763 5 3 1 48 73.57 2.43 1.2874 6 2 0 24 76.76 8.70 1.2417 5 3 3 24 81.99 5.74 1.1752 4 4 4 8 85.09 2.34 1.1401 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.