Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: M-Cr, 1st run, T = 400 C _database_code_amcsd 0008784 CELL PARAMETERS: 8.1265 8.1265 8.1265 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 536.674 Density (g/cm3): 3.605 MAX. ABS. INTENSITY / VOLUME**2: 19.46448951 RIR: 1.758 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.91 40.11 4.6918 1 1 1 8 31.13 31.56 2.8732 2 2 0 12 36.68 100.00 2.4502 3 1 1 24 44.60 56.79 2.0316 4 0 0 6 55.39 8.21 1.6588 4 2 2 24 59.07 2.84 1.5639 3 3 3 8 59.07 43.03 1.5639 5 1 1 24 64.91 67.48 1.4366 4 4 0 12 68.28 3.78 1.3736 5 3 1 48 73.74 2.37 1.2849 6 2 0 24 76.93 9.50 1.2393 5 3 3 24 77.99 1.26 1.2251 6 2 2 24 82.18 6.39 1.1730 4 4 4 8 85.29 3.03 1.1379 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.