Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: M-Cr, 1st run, T = 28 C _database_code_amcsd 0008785 CELL PARAMETERS: 8.1018 8.1018 8.1018 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 531.795 Density (g/cm3): 3.638 MAX. ABS. INTENSITY / VOLUME**2: 20.09451570 RIR: 1.799 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.97 40.08 4.6776 1 1 1 8 31.23 31.61 2.8644 2 2 0 12 36.79 100.00 2.4428 3 1 1 24 44.74 57.50 2.0254 4 0 0 6 55.57 8.50 1.6538 4 2 2 24 59.26 2.87 1.5592 3 3 3 8 59.26 45.07 1.5592 5 1 1 24 65.13 71.01 1.4322 4 4 0 12 68.52 3.95 1.3695 5 3 1 48 74.00 2.53 1.2810 6 2 0 24 77.21 10.22 1.2355 5 3 3 24 78.27 1.27 1.2214 6 2 2 24 82.48 6.93 1.1694 4 4 4 8 85.61 3.36 1.1345 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.