Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: M-Cr, 3rd run, T = 800 C _database_code_amcsd 0008792 CELL PARAMETERS: 8.1577 8.1577 8.1577 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 542.879 Density (g/cm3): 3.563 MAX. ABS. INTENSITY / VOLUME**2: 18.91579399 RIR: 1.728 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.84 35.51 4.7098 1 1 1 8 31.01 30.87 2.8842 2 2 0 12 36.53 100.00 2.4596 3 1 1 24 44.42 54.56 2.0394 4 0 0 6 55.16 8.15 1.6652 4 2 2 24 58.82 3.11 1.5699 3 3 3 8 58.82 38.20 1.5699 5 1 1 24 64.63 62.39 1.4421 4 4 0 12 67.98 2.98 1.3789 5 3 1 48 73.41 2.41 1.2898 6 2 0 24 76.59 8.47 1.2440 5 3 3 24 77.64 1.03 1.2298 6 2 2 24 81.80 5.44 1.1775 4 4 4 8 84.89 2.13 1.1423 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.