Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: M-Cr, 3rd run, T = 900 C _database_code_amcsd 0008793 CELL PARAMETERS: 8.1658 8.1658 8.1658 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 544.498 Density (g/cm3): 3.553 MAX. ABS. INTENSITY / VOLUME**2: 18.74545474 RIR: 1.718 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.82 34.52 4.7145 1 1 1 8 30.97 30.60 2.8870 2 2 0 12 36.49 100.00 2.4621 3 1 1 24 44.37 53.97 2.0415 4 0 0 6 55.10 8.02 1.6668 4 2 2 24 58.75 3.19 1.5715 3 3 3 8 58.75 36.85 1.5715 5 1 1 24 64.56 60.65 1.4435 4 4 0 12 67.91 2.90 1.3803 5 3 1 48 73.32 2.35 1.2911 6 2 0 24 76.50 8.19 1.2453 5 3 3 24 77.55 1.08 1.2310 6 2 2 24 81.70 5.22 1.1786 4 4 4 8 84.79 1.97 1.1434 5 5 1 24 89.90 3.48 1.0912 6 4 2 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.