Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: H-Cr, 3rd run, T = 550 C _database_code_amcsd 0008803 CELL PARAMETERS: 8.1445 8.1445 8.1445 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 540.248 Density (g/cm3): 3.606 MAX. ABS. INTENSITY / VOLUME**2: 19.51558960 RIR: 1.762 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.87 42.84 4.7022 1 1 1 8 31.06 31.01 2.8795 2 2 0 12 36.59 100.00 2.4557 3 1 1 24 44.50 57.82 2.0361 4 0 0 6 55.25 7.78 1.6625 4 2 2 24 58.92 42.98 1.5674 5 1 1 24 58.92 2.69 1.5674 3 3 3 8 64.75 66.82 1.4398 4 4 0 12 68.11 4.10 1.3767 5 3 1 48 73.55 2.14 1.2878 6 2 0 24 76.73 9.21 1.2420 5 3 3 24 77.79 1.24 1.2278 6 2 2 24 81.96 6.53 1.1756 4 4 4 8 85.06 3.23 1.1405 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.