Spinel Martignago F, Dal Negro A, Carbonin S Physics and Chemistry of Minerals 30 (2003) 401-408 How Cr3+ and Fe3+ affect Mg-Al order-disorder transformation at high temperature in natural spinels Sample: H-Cr, 3rd run, T = 600 C _database_code_amcsd 0008804 CELL PARAMETERS: 8.1482 8.1482 8.1482 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 540.985 Density (g/cm3): 3.601 MAX. ABS. INTENSITY / VOLUME**2: 19.44005886 RIR: 1.758 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.86 42.39 4.7044 1 1 1 8 31.04 30.87 2.8808 2 2 0 12 36.58 100.00 2.4568 3 1 1 24 44.48 56.97 2.0371 4 0 0 6 55.23 7.73 1.6632 4 2 2 24 58.89 2.77 1.5681 3 3 3 8 58.89 42.06 1.5681 5 1 1 24 64.72 65.25 1.4404 4 4 0 12 68.07 4.00 1.3773 5 3 1 48 73.51 2.14 1.2883 6 2 0 24 76.69 9.06 1.2426 5 3 3 24 77.74 1.38 1.2284 6 2 2 24 81.91 6.25 1.1761 4 4 4 8 85.01 3.04 1.1410 5 5 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.