Srilankite Troitzsch U, Christy A G, Ellis D J Physics and Chemistry of Minerals 32 (2005) 504-514 The crystal structure of disordered (Zr,Ti)O2 solid solution Sample: XTi = 0.666 _database_code_amcsd 0008989 CELL PARAMETERS: 4.7112 5.4944 4.9962 90.000 90.000 90.000 SPACE GROUP: Pbcn X-RAY WAVELENGTH: 1.541838 Cell Volume: 129.328 Density (g/cm3): 4.845 MAX. ABS. INTENSITY / VOLUME**2: 76.56864554 RIR: 5.146 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 24.90 18.19 3.5765 1 1 0 4 30.74 100.00 2.9082 1 1 1 8 32.59 10.60 2.7472 0 2 0 2 35.95 8.35 2.4981 0 0 2 2 37.36 6.90 2.4073 0 2 1 4 38.21 3.90 2.3556 2 0 0 2 40.89 3.89 2.2070 1 0 2 4 42.15 9.25 2.1437 1 2 1 8 44.23 4.32 2.0480 1 1 2 8 49.30 8.79 1.8482 0 2 2 4 51.08 8.32 1.7882 2 2 0 4 53.46 17.36 1.7138 2 0 2 4 53.70 8.80 1.7070 1 3 0 4 54.50 14.42 1.6836 2 2 1 8 57.01 3.74 1.6153 1 3 1 8 61.41 12.03 1.5097 1 1 3 8 64.03 5.36 1.4541 2 2 2 8 64.47 10.29 1.4454 3 1 1 8 65.55 5.84 1.4241 0 2 3 4 66.32 7.49 1.4094 1 3 2 8 71.19 4.22 1.3245 0 4 1 4 73.25 1.28 1.2922 3 1 2 8 76.22 1.29 1.2491 0 0 4 2 80.58 1.70 1.1922 3 3 0 4 81.77 2.14 1.1778 4 0 0 2 83.79 3.97 1.1545 2 4 1 8 85.38 1.21 1.1370 0 2 4 4 87.13 2.89 1.1186 3 1 3 8 88.63 2.18 1.1035 2 0 4 4 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.