Sellaite Baur W H Acta Crystallographica 9 (1956) 515-520 Uber die verfeinerung der kristallstrukturbestimmung einiger vertreter des rutiltyps: TiO2, SnO2, GeO2 und MgF2 _database_code_amcsd 0009163 CELL PARAMETERS: 4.6250 4.6250 3.0520 90.000 90.000 90.000 SPACE GROUP: P4_2/mnm X-RAY WAVELENGTH: 1.541838 Cell Volume: 65.284 Density (g/cm3): 3.169 MAX. ABS. INTENSITY / VOLUME**2: 14.66195943 RIR: 1.507 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 27.27 100.00 3.2704 1 1 0 4 35.23 17.96 2.5474 1 0 1 8 40.42 82.47 2.2313 1 1 1 8 43.77 26.31 2.0684 2 1 0 8 53.52 70.02 1.7122 2 1 1 16 56.26 26.75 1.6352 2 2 0 4 60.69 16.10 1.5260 0 0 2 2 63.62 4.57 1.4626 3 1 0 8 64.67 2.22 1.4413 2 2 1 8 67.76 10.73 1.3829 1 1 2 8 68.14 33.54 1.3761 3 0 1 8 71.54 5.09 1.3189 3 1 1 16 77.78 4.63 1.2280 2 1 2 16 83.63 3.24 1.1562 4 0 0 4 86.83 3.71 1.1217 4 1 0 8 87.42 9.99 1.1156 2 2 2 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.