Dysprosium Spedding F H, Daane A H, Herrmann K W Acta Crystallographica 9 (1956) 559-563 The crystal structures and lattice parameters of high-purity scandium, yttrium and the rare earth metals Locality: synthetic Note: sample 99.8% pure _database_code_amcsd 0009175 CELL PARAMETERS: 3.5903 3.5903 5.6475 90.000 90.000 120.000 SPACE GROUP: P6_3/mmc X-RAY WAVELENGTH: 1.541838 Cell Volume: 63.045 Density (g/cm3): 8.559 MAX. ABS. INTENSITY / VOLUME**2: 573.2275735 RIR: 21.807 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 28.71 24.09 3.1093 1 0 0 6 31.69 24.62 2.8238 0 0 2 2 32.88 100.00 2.7238 1 0 1 12 43.28 14.73 2.0904 1 0 2 12 50.86 17.31 1.7952 1 1 0 6 57.20 17.21 1.6104 1 0 3 12 59.46 2.50 1.5546 2 0 0 6 61.18 18.02 1.5149 1 1 2 12 61.90 12.95 1.4989 2 0 1 12 66.19 2.25 1.4119 0 0 4 2 68.95 2.91 1.3619 2 0 2 12 73.69 2.29 1.2855 1 0 4 12 80.05 5.18 1.1987 2 0 3 12 84.14 2.94 1.1506 2 1 1 24 88.00 5.15 1.1098 1 1 4 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.