Macedonite Glazer A M, Mabud S A Acta Crystallographica B34 (1978) 1065-1070 Powder profile refinement of lead zirconate titanate at several temperatures. II. Pure PbTiO3 Locality: synthetic Sample: T = 25 C _database_code_amcsd 0009631 3.905 3.905 4.156 90 90 90 P4mm atom x y z Biso B(1,1) B(2,2) B(3,3) B(1,2) B(1,3) B(2,3) Pb 0 0 0 .706 .009017 .008853 .012448 0 0 0 Ti .5 .5 .539 .060 -.002131 -.002131 .010277 0 0 0 O1 .5 .5 .114 .351 .012952 .012952 .005934 0 0 0 O2 .5 0 .617 .477 .010165 -.005410 .013316 0 0 0