Fergusonite-(Ce) Skinner S J, Brooks I J E, Munnings C N Acta Crystallographica C60 (2004) i37-i39 Tetragonal CeNbO4 at 1073 K in air and in vacuo Locality: synthetic Sample: in air _database_code_amcsd 0010328 CELL PARAMETERS: 5.3769 5.3769 11.5951 90.000 90.000 90.000 SPACE GROUP: I4_1/a X-RAY WAVELENGTH: 1.541838 Cell Volume: 335.230 Density (g/cm3): 5.884 MAX. ABS. INTENSITY / VOLUME**2: 233.5327790 RIR: 12.923 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.19 2.59 4.8780 1 0 1 8 28.07 100.00 3.1794 1 1 2 8 30.85 13.64 2.8988 0 0 4 2 33.33 19.53 2.6885 2 0 0 4 38.22 2.78 2.3545 2 1 1 8 39.08 1.38 2.3052 1 1 4 8 42.45 1.10 2.1294 1 0 5 8 44.37 1.72 2.0417 1 2 3 8 46.04 27.27 1.9712 2 0 4 8 47.85 12.24 1.9010 2 2 0 4 53.17 13.82 1.7228 1 1 6 8 56.39 10.16 1.6316 3 1 2 8 56.39 12.35 1.6316 1 3 2 8 58.02 9.25 1.5897 2 2 4 8 64.27 1.50 1.4494 0 0 8 2 69.99 2.81 1.3442 4 0 0 4 74.30 5.08 1.2766 3 1 6 8 74.30 3.67 1.2766 1 3 6 8 74.35 4.71 1.2758 2 0 8 8 77.02 3.86 1.2381 3 3 2 8 78.42 3.44 1.2195 4 0 4 8 79.76 1.75 1.2023 2 4 0 4 79.76 1.71 1.2023 4 2 0 4 83.96 2.71 1.1526 2 2 8 8 87.92 2.51 1.1106 4 2 4 8 87.92 2.47 1.1106 2 4 4 8 88.07 2.52 1.1091 1 1 10 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.