Tungsten Wyckoff R W G Crystal Structures 1 (1963) 7-83 Second edition. Interscience Publishers, New York, New York Sample is formed when certain tungstates are electrolyzed _database_code_amcsd 0011261 CELL PARAMETERS: 5.0830 5.0830 5.0830 90.000 90.000 90.000 SPACE GROUP: Pm3n X-RAY WAVELENGTH: 1.541838 Cell Volume: 131.329 Density (g/cm3): 18.593 MAX. ABS. INTENSITY / VOLUME**2: 1109.159122 RIR: 19.424 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 35.32 34.70 2.5415 2 0 0 6 39.65 100.00 2.2732 2 1 0 24 43.62 75.48 2.0751 2 1 1 24 63.39 7.59 1.4673 2 2 2 8 66.30 19.59 1.4098 3 2 0 24 69.15 34.06 1.3585 3 2 1 48 74.70 13.25 1.2708 4 0 0 6 85.42 8.92 1.1366 4 2 0 24 88.06 16.51 1.1092 4 2 1 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.