Cu La1.85 O4 Sr0.15 Decroux M, Junod A, Bezinge A, Cattani D, Cors J, Jorda L, Stettler A, Francois M, Yvon K, Fischer O, Muller J Europhysics Letters 3 (1987) 1035-1040 Structure, Resistivity, Critical Field, Specific-Heat Jump at Tc, Meissner Effect, a.c. and d.c. Susceptibility of the High-Temperature Superconductor La2-x Srx Cu O4. _cod_database_code 1008481 _database_code_amcsd 0016380 CELL PARAMETERS: 3.7793 3.7793 13.2000 90.000 90.000 90.000 SPACE GROUP: I4/mmm X-RAY WAVELENGTH: 1.541838 Cell Volume: 188.537 Density (g/cm3): 7.004 MAX. ABS. INTENSITY / VOLUME**2: 175.8609637 RIR: 8.176 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 13.42 3.76 6.6000 0 0 2 2 24.50 18.22 3.6333 1 0 1 8 27.02 10.44 3.3000 0 0 4 2 31.20 100.00 2.8669 1 0 3 8 33.53 64.24 2.6724 1 1 0 4 41.03 10.93 2.2000 0 0 6 2 41.73 21.22 2.1643 1 0 5 8 43.58 22.32 2.0768 1 1 4 8 48.15 29.22 1.8896 2 0 0 4 53.99 9.99 1.6985 1 1 6 8 54.37 9.00 1.6873 1 0 7 8 54.75 3.28 1.6765 2 1 1 16 55.71 4.16 1.6500 0 0 8 2 56.08 4.65 1.6398 2 0 4 8 58.50 28.14 1.5778 2 1 3 16 65.07 8.32 1.4335 2 0 6 8 65.58 8.52 1.4234 2 1 5 16 66.61 5.62 1.4040 1 1 8 8 70.47 7.22 1.3362 2 2 0 4 75.54 5.50 1.2586 2 1 7 16 76.67 5.32 1.2429 2 0 8 8 76.99 1.57 1.2385 2 2 4 8 79.07 4.95 1.2111 3 0 3 8 80.34 6.89 1.1951 3 1 0 8 81.29 1.17 1.1835 1 1 10 8 84.76 6.52 1.1437 1 0 11 8 84.91 3.22 1.1420 2 2 6 8 85.38 1.69 1.1370 3 0 5 8 86.64 3.84 1.1237 3 1 4 16 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.