Eskolaite Finger L W, Hazen R M Journal of Applied Physics 51 (1980) 5362-5367 Crystal structure and isothermal compression of Fe2O3, Cr2O3, and V2O3 to 50 kbars Locality: synthetic Note: P = 18.6 kbar _database_code_amcsd 0017738 CELL PARAMETERS: 4.9371 4.9371 13.5300 90.000 90.000 120.000 SPACE GROUP: R-3c X-RAY WAVELENGTH: 1.541838 Cell Volume: 285.609 Density (g/cm3): 5.301 MAX. ABS. INTENSITY / VOLUME**2: 38.72158361 RIR: 2.378 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 24.63 69.82 3.6143 0 1 2 6 33.79 100.00 2.6528 1 0 4 6 36.40 92.71 2.4685 1 1 0 6 39.98 6.38 2.2550 0 0 6 2 41.71 28.63 2.1654 1 1 3 12 44.44 5.59 2.0385 2 0 2 6 50.50 37.87 1.8071 0 2 4 6 55.17 87.36 1.6649 1 1 6 12 58.71 1.63 1.5727 0 1 8 6 58.74 5.81 1.5718 1 2 2 12 63.83 29.37 1.4582 2 1 4 12 65.49 38.38 1.4252 3 0 0 6 73.40 14.59 1.2900 1 0 10 6 73.80 2.76 1.2840 1 1 9 12 77.30 2.66 1.2343 2 2 0 6 79.57 2.87 1.2048 0 3 6 6 79.57 2.87 1.2048 3 0 6 6 82.60 1.12 1.1680 3 1 2 12 84.80 7.41 1.1433 0 2 10 6 86.27 1.98 1.1275 0 0 12 2 87.08 2.54 1.1191 1 3 4 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.