Eskolaite Finger L W, Hazen R M Journal of Applied Physics 51 (1980) 5362-5367 Crystal structure and isothermal compression of Fe2O3, Cr2O3, and V2O3 to 50 kbars Locality: synthetic Note: P = 56.8 kbar _database_code_amcsd 0017740 CELL PARAMETERS: 4.9128 4.9128 13.4689 90.000 90.000 120.000 SPACE GROUP: R-3c X-RAY WAVELENGTH: 1.541838 Cell Volume: 281.528 Density (g/cm3): 5.378 MAX. ABS. INTENSITY / VOLUME**2: 38.87082266 RIR: 2.353 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 24.75 74.01 3.5969 0 1 2 6 33.95 100.00 2.6404 1 0 4 6 36.58 95.02 2.4564 1 1 0 6 40.17 6.43 2.2448 0 0 6 2 41.92 29.32 2.1549 1 1 3 12 44.67 5.30 2.0285 2 0 2 6 50.76 39.95 1.7985 0 2 4 6 55.45 90.50 1.6571 1 1 6 12 57.74 1.08 1.5968 2 1 1 12 59.00 1.80 1.5655 0 1 8 6 59.06 5.75 1.5641 1 2 2 12 64.18 31.12 1.4511 2 1 4 12 65.86 39.85 1.4182 3 0 0 6 73.79 15.58 1.2841 1 0 10 6 74.20 3.01 1.2780 1 1 9 12 77.76 2.81 1.2282 2 2 0 6 80.03 3.04 1.1990 0 3 6 6 80.03 3.04 1.1990 3 0 6 6 83.10 1.27 1.1623 3 1 2 12 85.29 7.75 1.1380 0 2 10 6 86.76 2.18 1.1224 0 0 12 2 87.62 2.62 1.1136 1 3 4 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.