Cd Mo O4 Daturi M, Busca G, Borel M, Leclaire A, Piaggio P Journal of Physical Chemistry 101 (1997) 4358-4369 Vibrational and XRD study of the system Cd W O4 - Cd Mo O4 _cod_database_code 1001800 _database_code_amcsd 0013150 CELL PARAMETERS: 5.1560 5.1560 11.1960 90.000 90.000 90.000 SPACE GROUP: I4_1/a X-RAY WAVELENGTH: 1.541838 Cell Volume: 297.638 Density (g/cm3): 6.077 MAX. ABS. INTENSITY / VOLUME**2: 230.0264740 RIR: 12.325 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 29.23 100.00 3.0551 1 1 2 8 31.97 13.68 2.7990 0 0 4 2 34.80 18.35 2.5780 2 0 0 4 39.92 1.77 2.2584 2 1 1 8 40.64 1.83 2.2202 1 1 4 8 46.28 1.11 1.9616 1 2 3 8 47.98 26.89 1.8962 2 0 4 8 50.04 12.04 1.8229 2 2 0 4 55.31 13.54 1.6611 1 1 6 8 59.01 9.44 1.5654 3 1 2 8 59.01 12.17 1.5654 1 3 2 8 60.62 9.00 1.5275 2 2 4 8 66.85 1.35 1.3995 0 0 8 2 73.46 2.74 1.2890 4 0 0 4 77.63 4.99 1.2300 2 0 8 8 77.79 5.38 1.2278 3 1 6 8 77.79 3.51 1.2278 1 3 6 8 80.95 3.90 1.1876 3 3 2 8 82.36 3.44 1.1708 4 0 4 8 83.93 1.83 1.1529 2 4 0 4 83.93 1.73 1.1529 4 2 0 4 87.97 2.70 1.1101 2 2 8 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.