Khatyrkite Meetsma A, de Boer J L, van Smaalen S Journal of Solid State Chemistry 83 (1989) 370-372 Refinement of the crystal structure of tetragonal Al2Cu Locality: synthetic _database_code_amcsd 0013668 CELL PARAMETERS: 6.0670 6.0670 4.8770 90.000 90.000 90.000 SPACE GROUP: I4/mcm X-RAY WAVELENGTH: 1.541838 Cell Volume: 179.515 Density (g/cm3): 4.347 MAX. ABS. INTENSITY / VOLUME**2: 46.64823342 RIR: 3.494 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 20.70 100.00 4.2900 1 1 0 4 29.44 33.40 3.0335 2 0 0 4 37.95 48.81 2.3710 2 1 1 16 42.13 32.29 2.1450 2 2 0 4 42.65 74.13 2.1200 1 1 2 8 47.38 70.23 1.9186 3 1 0 8 47.86 58.36 1.9006 2 0 2 8 57.20 14.09 1.6106 2 2 2 8 61.10 1.64 1.5167 4 0 0 4 61.50 9.57 1.5078 3 1 2 16 66.36 5.16 1.4087 4 1 1 16 67.12 7.60 1.3945 2 1 3 16 69.26 13.78 1.3566 4 2 0 8 73.54 17.78 1.2879 4 0 2 8 77.36 20.00 1.2335 3 3 2 8 78.44 4.89 1.2192 0 0 4 2 80.77 4.40 1.1898 5 1 0 8 81.13 6.71 1.1855 4 2 2 16 82.19 3.06 1.1728 1 1 4 8 85.91 2.12 1.1313 2 0 4 8 89.22 4.09 1.0977 5 2 1 16 89.93 1.96 1.0909 4 1 3 16 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.