Tenorite Calos N J, Forrester J S, Schaffer G B Journal of Solid State Chemistry 122 (1996) 273-280 A crystallographic contribution to the mechanism of a mechanically induced solid state reaction Note: milling time = 32 min Locality: synthetic _database_code_amcsd 0018817 CELL PARAMETERS: 4.6844 3.4792 5.1215 90.000 98.684 90.000 SPACE GROUP: C2/c X-RAY WAVELENGTH: 1.541838 Cell Volume: 82.513 Density (g/cm3): 6.402 MAX. ABS. INTENSITY / VOLUME**2: 80.10817827 RIR: 4.074 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 32.18 5.24 2.7816 1 1 0 4 35.38 100.00 2.5369 -1 1 1 4 35.46 37.39 2.5314 0 0 2 2 38.31 99.66 2.3496 1 1 1 4 38.90 29.24 2.3154 2 0 0 2 49.15 25.36 1.8535 -2 0 2 2 52.61 12.75 1.7396 0 2 0 2 57.89 13.39 1.5929 2 0 2 2 61.64 18.42 1.5046 -1 1 3 4 65.06 16.09 1.4337 0 2 2 4 66.27 13.88 1.4104 -3 1 1 4 67.33 14.00 1.3908 2 2 0 4 67.47 11.64 1.3881 1 1 3 4 71.90 9.20 1.3131 3 1 1 4 74.86 7.46 1.2684 -2 2 2 4 75.05 4.66 1.2657 0 0 4 2 80.86 2.80 1.1887 -2 0 4 2 82.02 5.48 1.1748 2 2 2 4 82.91 5.56 1.1644 -3 1 3 4 83.51 3.11 1.1577 4 0 0 2 87.13 2.23 1.1186 -4 0 2 2 88.30 5.07 1.1068 -1 3 1 4 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.