Bi0.775 O1.5 Sm0.225 Drache M, Obbade S, Wignacourt J, Conflant P Journal of Solid State Chemistry 142 (1999) 349-359 Structural and conductivity properties of Bi(0.775) Ln(0.225) O1.5 oxide conductors (Ln = La, Pr, Nd, Sm, Eu, Gd, Tb, Dy) with rhombohedral Bi-Sr-O type _cod_database_code 1004138 _database_code_amcsd 0013962 CELL PARAMETERS: 3.9783 3.9783 27.3910 90.000 90.000 120.000 SPACE GROUP: R-3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 375.434 Density (g/cm3): 8.748 MAX. ABS. INTENSITY / VOLUME**2: 316.7022294 RIR: 11.788 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 19.44 2.86 4.5652 0 0 6 2 26.07 27.10 3.4184 1 0 1 6 26.68 26.14 3.3412 0 1 2 6 29.01 100.00 3.0777 1 0 4 6 29.35 48.98 3.0434 0 0 9 2 30.65 58.26 2.9165 0 1 5 6 34.69 8.00 2.5858 1 0 7 6 37.02 12.23 2.4286 0 1 8 6 42.15 6.01 2.1441 1 0 10 6 44.91 5.80 2.0182 0 1 11 6 45.61 46.51 1.9892 1 1 0 6 50.02 1.23 1.8236 1 1 6 12 50.79 25.14 1.7975 1 0 13 6 53.28 3.30 1.7193 0 2 1 6 53.62 3.39 1.7092 2 0 2 6 53.89 10.53 1.7013 0 1 14 6 54.96 14.50 1.6706 0 2 4 6 55.16 42.30 1.6651 1 1 9 12 55.95 9.66 1.6433 2 0 5 6 58.55 1.66 1.5766 0 2 7 6 60.13 2.71 1.5389 2 0 8 6 60.38 1.13 1.5331 1 0 16 6 60.88 4.07 1.5217 0 0 18 2 63.77 3.76 1.4595 0 1 17 6 63.83 1.39 1.4582 0 2 10 6 65.94 1.66 1.4167 2 0 11 6 69.93 1.40 1.3452 1 1 15 12 70.63 7.80 1.3336 0 2 13 6 72.69 2.22 1.3007 2 1 1 12 72.98 2.35 1.2964 1 2 2 12 73.21 3.60 1.2929 2 0 14 6 74.12 10.16 1.2793 2 1 4 12 74.96 7.09 1.2669 1 2 5 12 77.21 1.32 1.2356 2 1 7 12 78.60 2.19 1.2171 1 2 8 12 79.26 9.81 1.2086 1 1 18 12 81.86 1.61 1.1767 2 0 17 6 81.92 1.13 1.1761 2 1 10 12 82.35 4.75 1.1709 1 0 22 6 83.84 1.51 1.1539 1 2 11 12 84.33 5.46 1.1484 3 0 0 6 86.46 2.01 1.1256 0 1 23 6 88.21 7.55 1.1077 2 1 13 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.