Bi0.775 Gd0.225 O1.5 Drache M, Obbade S, Wignacourt J, Conflant P Journal of Solid State Chemistry 142 (1999) 349-359 Structural and conductivity properties of Bi(0.775) Ln(0.225) O1.5 oxide conductors (Ln = La, Pr, Nd, Sm, Eu, Gd, Tb, Dy) with rhombohedral Bi-Sr-O type _cod_database_code 1004140 _database_code_amcsd 0013964 CELL PARAMETERS: 3.9724 3.9724 27.3390 90.000 90.000 120.000 SPACE GROUP: R-3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 373.610 Density (g/cm3): 8.853 MAX. ABS. INTENSITY / VOLUME**2: 331.4641219 RIR: 12.192 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 19.48 3.47 4.5565 0 0 6 2 26.11 28.19 3.4133 1 0 1 6 26.72 24.94 3.3362 0 1 2 6 29.06 100.00 3.0729 1 0 4 6 29.40 44.87 3.0377 0 0 9 2 30.70 54.90 2.9118 0 1 5 6 34.75 7.11 2.5815 1 0 7 6 37.08 13.40 2.4245 0 1 8 6 42.22 5.64 2.1403 1 0 10 6 45.00 4.85 2.0146 0 1 11 6 45.68 45.17 1.9862 1 1 0 6 50.10 1.43 1.8207 1 1 6 12 50.89 24.81 1.7943 1 0 13 6 53.37 3.41 1.7167 0 2 1 6 53.71 3.20 1.7066 2 0 2 6 53.99 10.53 1.6983 0 1 14 6 55.05 14.46 1.6681 0 2 4 6 55.26 39.21 1.6624 1 1 9 12 56.05 9.15 1.6408 2 0 5 6 58.65 1.47 1.5742 0 2 7 6 60.23 2.95 1.5364 2 0 8 6 60.50 1.14 1.5303 1 0 16 6 61.00 3.87 1.5188 0 0 18 2 63.90 4.33 1.4569 0 1 17 6 63.95 1.29 1.4559 0 2 10 6 66.06 1.41 1.4144 2 0 11 6 70.07 1.45 1.3429 1 1 15 12 70.76 7.72 1.3314 0 2 13 6 72.82 2.28 1.2988 2 1 1 12 73.11 2.21 1.2944 1 2 2 12 73.35 3.56 1.2908 2 0 14 6 74.25 10.12 1.2774 2 1 4 12 75.10 6.73 1.2650 1 2 5 12 77.35 1.17 1.2337 2 1 7 12 78.74 2.37 1.2153 1 2 8 12 79.43 9.34 1.2065 1 1 18 12 82.03 1.84 1.1747 2 0 17 6 82.07 1.05 1.1742 2 1 10 12 82.54 4.55 1.1688 1 0 22 6 84.00 1.30 1.1521 1 2 11 12 84.49 5.31 1.1467 3 0 0 6 86.66 1.73 1.1235 0 1 23 6 88.38 7.48 1.1059 2 1 13 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.