Baddeleyite Kisi E H, Howard C J, Hill R J Journal of the American Ceramic Society 72 (1989) 1757-1760 Crystal structure of orthorhombic zirconia in partially stabilized zirconia Note: distorted polymorph of baddeleyite _database_code_amcsd 0014064 CELL PARAMETERS: 5.0680 5.2600 5.0770 90.000 90.000 90.000 SPACE GROUP: Pbc2_1 X-RAY WAVELENGTH: 1.541838 Cell Volume: 135.341 Density (g/cm3): 6.047 MAX. ABS. INTENSITY / VOLUME**2: 176.4148514 RIR: 9.500 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 17.50 1.58 5.0680 1 0 0 2 24.39 3.99 3.6496 1 1 0 4 30.16 100.00 2.9634 1 1 1 4 34.09 10.39 2.6300 0 2 0 2 35.36 11.41 2.5385 0 0 2 1 35.42 8.76 2.5340 2 0 0 2 38.55 2.17 2.3353 0 2 1 2 42.63 1.79 2.1209 1 2 1 4 43.42 1.90 2.0840 1 1 2 4 43.46 2.74 2.0821 2 1 1 4 49.93 15.44 1.8265 0 2 2 2 49.98 14.65 1.8248 2 2 0 4 50.92 16.04 1.7934 2 0 2 2 53.31 1.22 1.7183 1 2 2 4 53.35 3.72 1.7172 2 2 1 4 55.45 3.29 1.6570 1 3 0 4 58.60 11.83 1.5752 1 3 1 4 60.28 14.48 1.5353 1 1 3 4 60.37 13.79 1.5333 3 1 1 4 62.70 7.61 1.4817 2 2 2 4 65.60 1.32 1.4232 0 2 3 2 67.50 2.44 1.3875 1 3 2 4 71.78 1.08 1.3150 0 4 0 2 74.54 1.84 1.2730 0 4 1 2 74.80 1.90 1.2693 0 0 4 1 74.96 1.70 1.2670 4 0 0 2 81.25 3.69 1.1840 1 3 3 4 81.33 3.22 1.1830 3 3 1 4 82.64 1.17 1.1676 0 4 2 2 82.67 1.29 1.1672 2 4 0 4 82.79 4.13 1.1659 3 1 3 4 84.82 1.76 1.1431 0 2 4 2 84.97 1.55 1.1414 4 2 0 4 85.33 2.18 1.1375 2 4 1 4 85.58 2.19 1.1348 2 0 4 2 85.69 1.77 1.1336 4 0 2 2 89.29 1.64 1.0971 3 3 2 4 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.