Cu La2 O4 Chaillout C, Bordet P, Chenavas J, Cheong S, Fisk Z, Marezio M, Morosin B, Schirber J Materials Research Society Symposia Proceedings 169 (1990) 47-52 Structural aspects of the phase separation in La2CuO4.032 _cod_database_code 1008572 _database_code_amcsd 0016463 CELL PARAMETERS: 5.3500 13.1480 5.3980 90.000 90.000 90.000 SPACE GROUP: Cmca X-RAY WAVELENGTH: 1.541838 Cell Volume: 379.705 Density (g/cm3): 7.090 MAX. ABS. INTENSITY / VOLUME**2: 195.4046935 RIR: 8.974 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 13.47 3.12 6.5740 0 2 0 2 24.38 19.81 3.6505 1 1 1 8 27.13 11.07 3.2870 0 4 0 2 31.15 100.00 2.8710 1 3 1 8 33.19 31.70 2.6990 0 0 2 2 33.50 31.88 2.6750 2 0 0 2 41.20 10.47 2.1913 0 6 0 2 41.77 20.96 2.1623 1 5 1 8 43.38 12.45 2.0859 0 4 2 4 43.62 12.39 2.0748 2 4 0 4 47.88 30.56 1.8999 2 0 2 4 53.89 5.26 1.7012 0 6 2 4 54.10 5.37 1.6952 2 6 0 4 54.23 2.42 1.6913 1 1 3 8 54.50 10.76 1.6838 1 7 1 8 54.65 2.31 1.6794 3 1 1 8 55.90 6.20 1.6449 2 4 2 8 55.95 4.61 1.6435 0 8 0 2 58.03 17.21 1.5894 1 3 3 8 58.43 16.38 1.5795 3 3 1 8 64.96 8.98 1.4355 2 6 2 8 65.20 4.56 1.4309 1 5 3 8 65.57 4.76 1.4237 3 5 1 8 66.62 3.69 1.4037 0 8 2 4 66.81 3.59 1.4003 2 8 0 4 69.68 4.20 1.3495 0 0 4 2 70.39 4.38 1.3375 4 0 0 2 75.26 3.99 1.2626 1 7 3 8 75.61 4.06 1.2577 3 7 1 8 76.27 1.26 1.2484 0 4 4 4 76.66 7.02 1.2430 2 8 2 8 76.97 1.31 1.2389 4 4 0 4 78.62 6.92 1.2168 3 3 3 8 79.56 4.34 1.2049 2 0 4 4 80.07 4.53 1.1984 4 0 2 4 84.27 1.89 1.1491 0 6 4 4 84.95 2.01 1.1416 4 6 0 4 85.00 2.04 1.1411 3 5 3 8 85.08 8.78 1.1402 1 11 1 8 85.92 3.08 1.1313 2 4 4 8 86.42 3.15 1.1259 4 4 2 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.