IMA2010-039 Baldinozzi G, Berar J, Calvarin G Materials Science Forum 278 (1998) 680-685 Rietveld refinement of two-phase Zr-doped Y2 O3 _cod_database_code 1009017 _database_code_amcsd 0016879 CELL PARAMETERS: 10.5818 10.5818 10.5818 90.000 90.000 90.000 SPACE GROUP: Ia3 X-RAY WAVELENGTH: 1.541838 Cell Volume: 1184.892 Density (g/cm3): 5.063 MAX. ABS. INTENSITY / VOLUME**2: 141.8926820 RIR: 9.126 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 20.56 11.83 4.3200 2 1 1 24 29.24 100.00 3.0547 2 2 2 8 33.89 24.80 2.6455 4 0 0 6 36.01 4.72 2.4942 4 1 1 24 39.96 5.40 2.2560 3 3 2 24 43.61 3.50 2.0753 4 3 1 24 43.61 4.21 2.0753 4 1 3 24 47.04 1.11 1.9320 5 2 1 24 47.04 1.25 1.9320 5 1 2 24 48.68 39.59 1.8706 4 4 0 12 50.28 1.91 1.8148 4 3 3 24 53.37 2.88 1.7166 6 1 1 24 56.35 1.52 1.6328 5 4 1 24 56.35 1.97 1.6328 5 1 4 24 57.80 24.76 1.5953 6 2 2 24 59.22 2.48 1.5602 6 3 1 24 59.22 2.66 1.5602 6 1 3 24 60.63 3.97 1.5274 4 4 4 8 64.74 1.11 1.4400 7 2 1 24 71.30 3.51 1.3227 8 0 0 6 72.58 1.28 1.3025 8 1 1 24 78.86 5.65 1.2138 6 6 2 24 81.33 1.73 1.1831 8 0 4 12 81.33 1.73 1.1831 8 4 0 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.