Dy2 O3 Zachariasen W Norsk Geologisk Tidsskrift 9 (1927) 310-316 The crystal structure of the modification C of the sesquioxides of the rare earth metals, and of indium and thallium. _cod_database_code 1010336 _database_code_amcsd 0017262 CELL PARAMETERS: 10.6300 10.6300 10.6300 90.000 90.000 90.000 SPACE GROUP: I2_13 X-RAY WAVELENGTH: 1.541838 Cell Volume: 1201.157 Density (g/cm3): 8.249 MAX. ABS. INTENSITY / VOLUME**2: 438.9416137 RIR: 17.326 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 20.47 2.85 4.3397 2 1 1 12 29.10 100.00 3.0686 2 2 2 4 31.49 3.82 2.8410 3 2 1 12 31.49 3.95 2.8410 3 1 2 12 33.73 34.08 2.6575 4 0 0 6 35.84 4.84 2.5055 4 1 1 12 39.77 1.36 2.2663 3 3 2 12 43.41 4.13 2.0847 4 3 1 12 43.41 3.70 2.0847 4 1 3 12 46.81 2.58 1.9408 5 2 1 12 46.81 1.69 1.9408 5 1 2 12 48.44 34.63 1.8791 4 4 0 12 50.03 1.92 1.8230 4 3 3 12 53.11 3.17 1.7244 6 1 1 12 56.07 1.61 1.6402 5 4 1 12 56.07 1.54 1.6402 5 1 4 12 57.51 26.15 1.6025 6 2 2 12 58.93 1.68 1.5673 6 3 1 12 58.93 1.69 1.5673 6 1 3 12 60.32 5.03 1.5343 4 4 4 4 61.70 1.12 1.5033 5 4 3 12 64.41 1.20 1.4466 6 3 3 12 65.74 1.20 1.4205 6 4 2 12 70.93 3.37 1.3288 8 0 0 6 78.43 5.76 1.2193 6 6 2 12 80.88 2.15 1.1885 8 0 4 12 80.88 2.15 1.1885 8 4 0 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.