O3 Tb2 Zachariasen W Norsk Geologisk Tidsskrift 9 (1927) 310-316 The crystal structure of the modification C of the sesquioxides of the rare earth metals, and of indium and Thallium. _cod_database_code 1010337 _database_code_amcsd 0017263 CELL PARAMETERS: 10.7000 10.7000 10.7000 90.000 90.000 90.000 SPACE GROUP: I2_13 X-RAY WAVELENGTH: 1.541838 Cell Volume: 1225.043 Density (g/cm3): 7.933 MAX. ABS. INTENSITY / VOLUME**2: 413.7355091 RIR: 16.981 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 20.33 2.78 4.3683 2 1 1 12 28.91 100.00 3.0888 2 2 2 4 31.28 3.84 2.8597 3 2 1 12 31.28 3.98 2.8597 3 1 2 12 33.50 33.80 2.6750 4 0 0 6 35.60 4.82 2.5220 4 1 1 12 39.50 1.36 2.2812 3 3 2 12 43.11 4.15 2.0984 4 3 1 12 43.11 3.72 2.0984 4 1 3 12 46.49 2.62 1.9535 5 2 1 12 46.49 1.71 1.9535 5 1 2 12 48.10 34.86 1.8915 4 4 0 12 49.68 1.91 1.8350 4 3 3 12 52.74 3.19 1.7358 6 1 1 12 55.67 1.61 1.6510 5 4 1 12 55.67 1.55 1.6510 5 1 4 12 57.10 26.19 1.6131 6 2 2 12 58.50 1.68 1.5776 6 3 1 12 58.50 1.69 1.5776 6 1 3 12 59.89 5.00 1.5444 4 4 4 4 61.26 1.12 1.5132 5 4 3 12 63.94 1.20 1.4561 6 3 3 12 65.25 1.21 1.4298 6 4 2 12 70.39 3.40 1.3375 8 0 0 6 77.82 5.77 1.2274 6 6 2 12 80.24 2.13 1.1963 8 4 0 12 80.24 2.13 1.1963 8 0 4 12 89.81 3.76 1.0921 8 4 4 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.