Iron Basinski Z S, Hume-Rothery W, Sutton A L Proceedings of the Royal Society of London A229 (1955) 459-467 The lattice expansion of iron Locality: synthetic Sample: at T = 1060 K _database_code_amcsd 0015344 CELL PARAMETERS: 2.8930 2.8930 2.8930 90.000 90.000 90.000 SPACE GROUP: Im3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 24.213 Density (g/cm3): 7.659 MAX. ABS. INTENSITY / VOLUME**2: 297.8621453 RIR: 12.664 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 44.28 100.00 2.0457 1 1 0 12 64.41 13.53 1.4465 2 0 0 6 81.50 23.73 1.1811 2 1 1 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.