Bunsenite Taguchi H Solid State Communications 108 (1998) 635-639 Relationship between crystal structure and electrical properties of murdochite-type Ni6+2xMn1-xO8 Locality: Synthetic Sample Number: x = 0.0 _database_code_amcsd 0015491 CELL PARAMETERS: 8.3200 8.3200 8.3200 90.000 90.000 90.000 SPACE GROUP: Fm3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 575.930 Density (g/cm3): 6.170 MAX. ABS. INTENSITY / VOLUME**2: 109.8342851 RIR: 5.796 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.47 19.89 4.8036 1 1 1 8 21.36 11.27 4.1600 2 0 0 6 30.39 9.04 2.9416 2 2 0 12 35.79 6.03 2.5086 3 1 1 24 37.44 65.72 2.4018 2 2 2 8 43.51 100.00 2.0800 4 0 0 6 47.64 1.34 1.9087 3 3 1 24 48.96 5.15 1.8604 4 2 0 24 53.99 3.67 1.6983 4 2 2 24 57.56 3.01 1.6012 5 1 1 24 63.22 54.82 1.4708 4 4 0 12 66.48 2.48 1.4063 5 3 1 48 67.55 1.91 1.3867 4 4 2 24 71.75 1.13 1.3155 6 2 0 24 75.85 24.74 1.2543 6 2 2 24 79.88 16.29 1.2009 4 4 4 8 82.86 1.10 1.1650 5 5 1 24 87.80 1.36 1.1118 6 4 2 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.